Mold Best Assurance Company Limited
Mold maintenance is more important than mold repair. The more mold is repaired, the shorter the life is; the better mold is maintained, the longer its service life will be.
Not only injection mold temperature determines melt temperature as it moves quickly through the mold. The melt temperature itself as it starts its journey through the injection mold (self-evidently) is the reference point. Speed of injection, particularly in thin sections, is of huge influence, as it will determine the degree of shear heating.
Many engineering materials like PBT (Polybutylene terephthalate) have a tendency of out-gassing. The best practices that I have to date are: Add 10mm wide vents spaced 30mm from each other all the way around parting line. Always follow the recommendations of the material company for vent depth.